Product introduction
Mixed Metal Oxide Anode is suitable for many environments, such as soil, fresh water, saline water and seawater. At present, it is the most promising product to replace high silicon cast iron anode in cathodic protection, with light weight, long service life and high cost performance.
- Product features:
- MMO tubular anode has a large specific surface area, so the current output is large and the anode grounding resistance is small.
- MMO tubular anodes can reduce installation costs by 15-35% compared to other anodes.
- The unique flexibility of MMO tubular anodes facilitates handling, transportation and installation.
Product Parameter
|
Technical Parameter |
|
|
Substrate |
Titanium ASTM B338 GR1 |
|
Coated element |
Mixed Metal Oxide |
|
Current output |
Soil 100A/m2 |
|
Sea water 600A/m2 |
|
|
Thermal expansion coefficient |
8.7*10-5/K |
|
Thermal conductivity |
15.6W/m.K |
|
Anode-to-Cable Resistance |
0.0009Ω |
|
Tensile strengths |
280MPa |
|
Pull-Out Strength of Cable-Anode Connection |
100kg |
Product Specification
|
Diameter(mm) |
Length(mm) |
Thickness(mm) |
Weight(kg) |
Surface area(m2) |
Maximum current output (A/m) |
Life(a) |
|
19 |
1200 |
1.0 |
0.305 |
0.072 |
7.2 |
20 |
|
25 |
500 |
1.5 |
0.249 |
0.039 |
4 |
20 |
|
25 |
1000 |
1.0 |
0.339 |
0.079 |
8 |
20 |
|
25 |
1000 |
1.5 |
0.498 |
0.079 |
8 |
20 |
|
25 |
1500 |
1.5 |
0.747 |
0.118 |
12 |
20 |
|
32 |
1200 |
2.0 |
1.02 |
0.121 |
12 |
20 |
*Based on 20-year design life in calcined petroleum grade coke.
Hot Tags: MMO tubular anode, China, suppliers, manufacturers, factory, cheap, GPS Current Interrupter, Canistered Cast Iron Anode, Zinc Alloy Cast Anode, Cu/CuSO4 Reference Electrode, MMO Ribbon Mesh Anode, Portable Transformer Rectifier